Carbon Steel 1022

 

Applications

1022 steel is typically used for moderate strength structural applications such as cold formed fasteners and bolts. It is often used in the case hardened condition

Forming

1022 steel has good ductility and is readily formed by conventional means.

Welding

Weldable by all standard methods. However for heavy sections the use of pre-heat and post- heat is advised.

Heat Treatment

1022 may be hardened by heating to 1500 - 1600 F and water quenching. The product should then be tempered. However for a low carbon steel such as this the improvement in strength from heat treat, quench and temper often are not cost effective in terms of the heat treating cost.

Forging

Forge at 2350 to 1800 F.

Hot Working

Hot work at 900 to 200 F.

Annealing

A full anneal is done at 1700 F with slow furnace cooling. A stress relief anneal may be done at 1000 F.

Aging

Not applicable.

Density: 0.284

Specific Gravity: 7.86

Melting Point: 2760

MoETensile: 30

 

To Send a Request for Quote, please Click Here, call , or fax (973) 276 - 5050

Announcements

Looking Ahead to Metals in 2010
For CEO's, Purchasing Agents, Engineers, Machine Shops, OEMs, Business Owners ...
ISM's Purchasing Managers Report posted 10:00 A.M. ET November 2nd, 2009 PMI is 55.7%.
White Papers

Search

Alloy Steels Aluminum Alloys Carbon Steels Copper Alloys Magnesium Alloys Nickel Alloys, Cobalt  Alloys, Special Alloys  and Super Alloys Refractory Alloys Stainless Steels &
 PH Grades
Titanium Alloys Tool Steels Zirconium
Forging Capabilities History of Forgings How To Buy How Forgings Are Made Cost Saving Tips